The galvanic effect in seawater should be minimal for the time that dissimilar metals are in contact. However, you might want a sacrificial anode -- perhaps a zinc casting of Neptune -- if there's any concern. Most divers of any persuasion wash down their rig with freshwater at the end of the day anyway. In water containing other chemicals (SO2 or black water) YMMV. For some users here, I'd advise a sacrificial anode made of cesium. ;) Jim Strohm PADI OWSI 51985