>Based on observations in the chemical industry involving oxygen >applications, the fact that every resource on materials compatibilty I have >ever seen says viton is superior to buna-n in oxygen service and the fact >that viton o-rings are only slightly more expensive than buna-n,if any at >all, I wonder, why not use viton? Viton does decompose at high temps to a sticky residue containing some sort of Flouric acid. We had a warning message sent round, stating that the only cure for skin contact was amputation of the affected area. I guess its ok as long as you know. Bill.Dyer@mi*.co*.uk*